Metallography · hardness · mechanics · optics — one chainMetallography & testing
National High-TechShanghai SME2 Patents
3 products
HOW IT WORKS

How it works

Typical process parametersHeating 150–180 °CPressure 20–30 MPaWater cooling 3–6 minDies Ø25–45 mmPressing ramHeating jacket + water coolingMachine body / control panel

Mounting encapsulates small, irregular or edge-critical specimens in resin so later grinding has a flat support and the edge does not round over. Hot mounting cures thermosetting resin at 150–180 °C and 20–30 MPa for 5–15 min, then demoulds after cooling; cold mounting uses epoxy or acrylic at room temperature for heat-sensitive materials. The ZHONGYAN ZXQ series integrates heating, pressing and water cooling, one or two specimens per cycle, with interchangeable Ø25–45 mm dies.

Heating + water coolingØ25–45 mm diesHot and cold routes
Generate a selection proposal
WORKFLOW

Standard workflow

The preparation/inspection workflow built around the Metallographic Mounting Presses — every step has its own consumables and parameters.

Workflow1SectioningCut the represent…2Load the dieInspection face d…3Heat & press150–180 °C at 20–…4CoolingWater cool 3–6 mi…5Demould & lab…Demould, number a…
SPECIFICATIONS

Key specifications

Die sizesØ 25 / 30 / 40 / 45 mm
Heating range0 – 200 °C
Pressing force0 – 30 MPa
Specimens per cycle1 – 2
CoolingBuilt-in water circuit
SELECTION

How to choose

  1. 1

    Many specimens needing consistency → intelligent automatic press with programmed temperature and pressure.

  2. 2

    Heat-sensitive aluminium alloys, quenched foils or coatings → cold mounting with epoxy, curing at room temperature without altering the structure.

  3. 3

    Conductive mounting for SEM/EBSD → use conductive resin with carbon or metal filler, or carbon-coat after mounting.

FAQ

FAQ

Gaps appear at the edge after mounting and coolant seeps in?
Resin shrinkage. Ramp the temperature in steps (120 °C then 175 °C), allow full holding time, or switch to low-shrinkage epoxy cold mounting.
The mount will not come out of the die?
Insufficient cooling or no release agent. Cool below 60 °C before demoulding, apply a thin release agent each cycle and keep powder resin dry.
Hot or cold mounting — which one?
For routine steels and batch work use hot mounting — fast and hard. For heat- or pressure-sensitive specimens, or when edge detail matters, use cold mounting. Running both gives the best throughput.
Compare tray 0/4