Standards and verification regulations

GB/T test methods, JJG verification regulations and ISO/ASTM international standards for hardness, metallography, dimensional metrology and environmental testing — 44 entries grouped by product line.

GB/TNational standard29 项

StandardTitleScope
GB/T 230.1 Metallic materials — Rockwell hardness test — Part 1: Test method Test method
GB/T 231.1 Metallic materials — Brinell hardness test — Part 1: Test method Test method
GB/T 4340.1 Metallic materials — Vickers hardness test — Part 1: Test method Test method
GB/T 17394.1 Metallic materials — Leeb hardness test — Part 1: Test method Test method
GB/T 18449.1 Metallic materials — Knoop hardness test — Part 1: Test method Test method
GB/T 21838.1 Metallic materials — Instrumented indentation test for hardness and materials parameters — Part 1: Test method Test method
GB/T 2611 Testing machines — General technical requirements Product standard
GB/T 16491 Electronic universal testing machines Product standard
GB/T 3159 Hydraulic universal testing machines Product standard
GB/T 3808 Verification of pendulum-type impact testing machines Product standard
GB/T 16825.1 Metallic materials — Calibration and verification of static uniaxial testing machines 检定依据
GB/T 1040.1 Plastics — Determination of tensile properties — Part 1: General principles Test method
GB/T 228.1 Metallic materials — Tensile testing — Part 1: Method of test at room temperature Test method
GB/T 229 Metallic materials — Charpy pendulum impact test method Test method
GB/T 13298 Inspection methods for microstructure of metallic materials Test method
GB/T 6394 Determination of estimating the average grain size of metal Test method
GB/T 10561 Steel — Determination of content of nonmetallic inclusions — Micrographic method Test method
GB/T 11354 Determination of nitrided case depth and metallographic examination Test method
GB/T 2985 Biological microscopes Product standard
GB/T 22058 Microscopes — Stereomicroscopes — Information provided to the user Product standard
GB/T 24762 GPS — Acceptance and reverification tests for imaging measuring instruments Product standard
GB/T 1957 Plain limit gauges — Technical specifications Product standard
GB/T 1800.1 GPS — ISO code system for tolerances on linear sizes Basic standard
GB/T 10592 Specifications for high/low temperature test chambers Product standard
GB/T 10125 Corrosion tests in artificial atmospheres — Salt spray tests Test method
GB/T 2423.1 Environmental testing — Part 2: Tests — Test A: Cold Test method
GB/T 4336 Carbon and low-alloy steel — Determination of multi-element contents — Spark discharge atomic emission spectrometric method Test method
GB/T 11170 Stainless steel — Determination of multi-element contents — Spark discharge atomic emission spectrometric method Test method
GB/T 4956 Non-magnetic coatings on magnetic substrates — Measurement of coating thickness — Magnetic method Test method

JJGNational verification regulation6 项

StandardTitleScope
JJG 112 Verification Regulation of Metallic Rockwell Hardness Testers Verification regulation
JJG 150 Verification Regulation of Metallic Brinell Hardness Testers Verification regulation
JJG 151 Verification Regulation of Metallic Vickers Hardness Testers Verification regulation
JJG 1047 Verification Regulation of Metallic Knoop Hardness Testers Verification regulation
JJG 747 Verification Regulation of Leeb Hardness Testers Verification regulation
JJG 202 Verification Regulation of Autocollimators Verification regulation

JJFNational calibration specification1 项

StandardTitleScope
JJF 1101 Calibration Specification for Temperature and Humidity Parameters of Environmental Test Chambers Calibration spec.

JB/TMachinery industry standard1 项

StandardTitleScope
JB/T 9324 Metallurgical microscopes Industry standard

NB/TEnergy industry standard1 项

StandardTitleScope
NB/T 47013.1 Nondestructive testing of pressure equipments — Part 1: General requirements Industry standard

ISOInternational standard3 项

StandardTitleScope
ISO 14577-1 Metallic materials — Instrumented indentation test for hardness and materials parameters 国际标准
ISO 6508-1 Metallic materials — Rockwell hardness test 国际标准
ISO 6507-1 Metallic materials — Vickers hardness test 国际标准

ASTMASTM standard3 项

StandardTitleScope
ASTM E2546 Standard Practice for Instrumented Indentation Testing 国际标准
ASTM E18 Standard Test Methods for Rockwell Hardness of Metallic Materials 国际标准
ASTM E384 Standard Test Method for Microindentation Hardness of Materials 国际标准

How to use

  • Always refer to the currently valid edition. Numbers here omit the year; state the edition year in purchase and acceptance documents.
  • JJG are verification regulations used for annual metrology inspection; GB/T are test-method or product standards used for acceptance and test reports.
  • Export projects often require ISO 6507/6508 together with ASTM E18/E384; matching calibration certificates ship with the machine.