Metallography · hardness · mechanics · optics — one chainMetallography & testing
National High-TechShanghai SME2 Patents
STANDARDS

Standards and verification regulations

GB/T test methods, JJG verification regulations and ISO/ASTM international standards for hardness, metallography, dimensional metrology and environmental testing — 44 entries grouped by product line.

GB/TNational standard6 项

StandardTitleScope
GB/T 230.1 Metallic materials — Rockwell hardness test — Part 1: Test method Test method
GB/T 231.1 Metallic materials — Brinell hardness test — Part 1: Test method Test method
GB/T 4340.1 Metallic materials — Vickers hardness test — Part 1: Test method Test method
GB/T 17394.1 Metallic materials — Leeb hardness test — Part 1: Test method Test method
GB/T 18449.1 Metallic materials — Knoop hardness test — Part 1: Test method Test method
GB/T 21838.1 Metallic materials — Instrumented indentation test for hardness and materials parameters — Part 1: Test method Test method

JJGNational verification regulation5 项

StandardTitleScope
JJG 112 Verification Regulation of Metallic Rockwell Hardness Testers Verification regulation
JJG 150 Verification Regulation of Metallic Brinell Hardness Testers Verification regulation
JJG 151 Verification Regulation of Metallic Vickers Hardness Testers Verification regulation
JJG 1047 Verification Regulation of Metallic Knoop Hardness Testers Verification regulation
JJG 747 Verification Regulation of Leeb Hardness Testers Verification regulation

ISOInternational standard3 项

StandardTitleScope
ISO 14577-1 Metallic materials — Instrumented indentation test for hardness and materials parameters 国际标准
ISO 6508-1 Metallic materials — Rockwell hardness test 国际标准
ISO 6507-1 Metallic materials — Vickers hardness test 国际标准

ASTMASTM standard3 项

StandardTitleScope
ASTM E2546 Standard Practice for Instrumented Indentation Testing 国际标准
ASTM E18 Standard Test Methods for Rockwell Hardness of Metallic Materials 国际标准
ASTM E384 Standard Test Method for Microindentation Hardness of Materials 国际标准

How to use

  • Always refer to the currently valid edition. Numbers here omit the year; state the edition year in purchase and acceptance documents.
  • JJG are verification regulations used for annual metrology inspection; GB/T are test-method or product standards used for acceptance and test reports.
  • Export projects often require ISO 6507/6508 together with ASTM E18/E384; matching calibration certificates ship with the machine.
Compare tray 0/4
Compare now