STANDARDS
Standards and verification regulations
GB/T test methods, JJG verification regulations and ISO/ASTM international standards for hardness, metallography, dimensional metrology and environmental testing — 44 entries grouped by product line.
GB/TNational standard3 项
| Standard | Title | Scope | |
|---|---|---|---|
| GB/T 4336 | Carbon and low-alloy steel — Determination of multi-element contents — Spark discharge atomic emission spectrometric method | Test method | Products |
| GB/T 11170 | Stainless steel — Determination of multi-element contents — Spark discharge atomic emission spectrometric method | Test method | Products |
| GB/T 4956 | Non-magnetic coatings on magnetic substrates — Measurement of coating thickness — Magnetic method | Test method | Products |
NB/TEnergy industry standard1 项
| Standard | Title | Scope | |
|---|---|---|---|
| NB/T 47013.1 | Nondestructive testing of pressure equipments — Part 1: General requirements | Industry standard | Products |
How to use
- Always refer to the currently valid edition. Numbers here omit the year; state the edition year in purchase and acceptance documents.
- JJG are verification regulations used for annual metrology inspection; GB/T are test-method or product standards used for acceptance and test reports.
- Export projects often require ISO 6507/6508 together with ASTM E18/E384; matching calibration certificates ship with the machine.