HR-150A/HRS-150 Rockwell Hardness Tester
Overview
No translation available yet — Chinese original below Full description (Chinese original) ↓
Measuring capability2
What it can measure — the first thing to check against your samples
- Test Force
- 588(60kg) 、980N(100kg)、1471N(150kg)
- 硬度测试范围
- HRA:20 ~88、HRB:20~100、HRC:20~70
Structure & travel2
Stage, travel, dimensions and weight — siting and fixturing
- Max Specimen Height
- 170mm
- Overall Dimensions
- 550 ×240×750mm
Loading & control2
Loading mode, speed, dwell and software interfaces
- Test force loading method
- Manual · automatic
- Dwell Time
- 0 – 60S
Power & environment2
Power, consumption and ambient requirements
- Power Supply
- 220V/50HZ
- Power supply 线
- 一根
Accessories & configuration3
Standard, optional and supplied-with items
- Main unit weight
- 100kg
- Main Unit
- 一台
- 打印纸
- 一包
Other9
Additional notes
- Reading Mode
- 表盘(金属) · 触摸屏数显
- 压头中心距离
- 165mm
- 砝码
- 三只
- 太 stage
- 一件
- 中 stage
- 一件
- V-type stage
- 一件
- 金刚石洛氏压头
- 一只
- 洛氏球压头
- 一只
- 洛氏硬度块
- 三块
Specifications vary with configuration — confirm the final technical agreement with our engineer. Optional items are priced separately.
| Test Force | 588(60kg) 、980N(100kg)、1471N(150kg) |
|---|---|
| Test force loading method | Manual · automatic |
| 硬度测试范围 | HRA:20 ~88、HRB:20~100、HRC:20~70 |
| Dwell Time | 0-60S |
| Reading Mode | 表盘(金属) · 触摸屏数显 |
| Max Specimen Height | 170mm |
| 压头中心距离 | 165mm |
| Overall Dimensions | 550 ×240×750mm |
| Main unit weight | 100kg |
| Power Supply | 220V/50HZ |
| Main Unit | 一台 |
| 砝码 | 三只 |
| 太 stage | 一件 |
| 中 stage | 一件 |
| V-type stage | 一件 |
| 金刚石洛氏压头 | 一只 |
| 洛氏球压头 | 一只 |
| 洛氏硬度块 | 三块 |
| 打印纸 | 一包 |
| Power supply 线 | 一根 |
Some specification values are given in the original Chinese wording; ask our engineers for an English datasheet.
Full description (Chinese original)
The English text on this page summarises the model and specifications. The full technical description is the Chinese original below; an English datasheet is available from our engineers on request.
产品介绍
适用于黑色金属、有色金属和非金属材料的硬度测定,如淬火、表面淬火钢,调质、退火钢,冷硬铸件,可锻铸件,硬质合金钢,铝合金,轴承钢,硬化薄钢板等.
产品特点
金相分析讲义-金相分析免费视频课程 :http://shanghaizhongyan.com/
Selection FAQ
Can the configuration of HR-150A/HRS-150 be adapted to my application?
Yes. Beyond the standard configuration, measuring range, fixtures, optics and software functions can be adapted. Send your sample and test requirements and our engineers will return a configuration list and quotation.
Can I test my samples before ordering?
Yes. Samples can be mailed to our Shanghai Fengxian laboratory for free testing with a written report, or you can book an on-site demonstration to confirm the workflow and data format.
How are lead time, installation and after-sales service handled?
Standard configurations usually ship within 15-30 working days, including first installation, commissioning and operator training. The instrument carries a one-year warranty and software upgrades are free for life.
General information only — final configuration and applicable conditions are subject to the mutually confirmed technical document.
同类工件怎么测
典型场景
AutomotiveCarburised gears: disputed case depthZHVST-30F micro-Vickers system with motorised stage;…GB/T 9450, ISO 2639BearingsRings: sampling rate cannot keep upHRS-150 digital Rockwell tester gives a direct HRC r…GB/T 230.1, GB/T 18254After-Sale & Selection Support
Sample Testing
- Free testing of mailed samples
- Factory demo by appointment
- Written test proposal provided
Delivery & Training
- Free first installation & commissioning
- On-site operation training
- One-year full warranty
Custom Builds
- Fixtures, ranges and software customizable
- Automation line integration
- Lifetime free software upgrades