Why the Mounted Specimen Cannot Be Removed from the Mounting Press
Articles in this section are published in Chinese. Contact us for English materials.
冷却不彻底或未涂脱模剂。冷却到 60 ℃ 以下再脱模;每次合模前薄涂脱模剂,模具内壁保持清洁;粉末树脂受潮会粘连,应密封干燥保存。树脂用量也要按模具容积给足,过多会顶死压头。