Metallography · hardness · mechanics · optics — one chainMetallography & testing
National High-TechShanghai SME2 Patents
FAQ

HR-150 Rockwell Hardness Tester Pointer Suddenly Rises or Falls at the End of Unloading

Articles in this section are published in Chinese. Contact us for English materials.

杠杆刀刃磨损或压头松动。检查刀刃刃口与压头紧固情况,磨损明显需更换杠杆或压头。