HR-150 Rockwell Hardness Tester A, B and C Scale Values Are Consistently Too High

Articles in this section are published in Chinese. Contact us for English materials.

压头磨损(球压头直径偏小)或总载荷偏大、测深零点偏移。用标准块验证后重校零点,更换合格压头。