Microstructure, Metallographic Analysis and Microstructure Explanation

Articles in this section are published in Chinese. Contact us for English materials.

金相组织分析的基本顺序:低倍观察宏观缺陷 → 中倍看组织类别与分布 → 高倍测晶粒度、层深与夹杂物级别。判定依据是 GB/T 6394(晶粒度)、GB/T 10561(夹杂物)、GB/T 13298(组织检验)等标准。