Precautions When Using the Metallographic Cutting Machine

Articles in this section are published in Chinese. Contact us for English materials.

① 试样必须夹紧,切割片与夹具不得干涉;② 冷却液液位与流量要足,喷嘴对准切口;③ 按材料硬度选切割片与转速,脆性与薄片件用低速薄片;④ 换片后先空转 30 s 确认无摆动;⑤ 切完及时清洗,防止磨屑进入导轨与水箱。