装盘 → 选砂纸 → 设定转速与单颗压力 → 开滴液 → 磨到上一道划痕完全消失 → 逐级换砂纸(320→600→1000/1200)→ 抛光(1–3 μm 金刚石)→ 清洗吹干 → 浸蚀 → 观察。每次换道都要清洗试样与手,磨盘转向与试样自转方向一致。