HR-150 Rockwell Hardness Tester Pointer Jitters After the Main Load Is Fully Applied
Articles in this section are published in Chinese. Contact us for English materials.
缓冲器(阻尼器)缺油或油路有气泡,或机架受外界振动。补足规定牌号缓冲油并排气,给设备加减振垫,避开冲压设备等振动源。
Articles in this section are published in Chinese. Contact us for English materials.
缓冲器(阻尼器)缺油或油路有气泡,或机架受外界振动。补足规定牌号缓冲油并排气,给设备加减振垫,避开冲压设备等振动源。